What makes superalloys super - hierarchical microstructure of a superalloy
by Staff Writers
Berlin, Germany (SPX) Jan 16, 2014


The image shows the three-dimensional reconstruction of an atom probe measurement. The matrix (purple) can be seen surrounding the cuboidal precipitates (green). Only a few nanometre-sized platelets can be seen in the precipitates. Atom probe tomography allows a site specific analysis of the structure at the atomic scale and reveals the chemical composition in measurements of individual areas. Image: HZB

Researchers have observed for the first time in detail how a hierarchical microstructure develops during heat treatment of a superalloy

Materials in high-performance turbines have to withstand not only powerful mechanical forces, they also have to maintain their chemical and mechanical properties almost up to their melting points. For this reason, turbine manufacturers have employed special nickel-based high-performance alloys for decades.

New work from Helmholtz-Zentrum Berlin fur Materialien and Energie (HZB) now shows in detail how new phases in a nickel-based alloy form and evolve, providing clues to how high-performance alloys could be improved.

Doctoral student Florian Vogel and Dr. Nelia Wanderka from the HZB Institute of Applied Materials have elegantly combined two methods to accomplish this: transmission electron microscopy (TEM) and atom probe tomography (APT), which they carried out in collaboration with colleagues from the University of Munster.

They were interested in a phase separation phenomenon that has been known for around 50 years, but could neither be precisely observed nor understood until now: The microstructure of nickel-based alloys changes under controlled ageing or heat treatment and in the classical two-phase microstructure new phases are initially formed. Wanderka and Vogel were able to precisely observe the phase separation process on the atomic scale for the first time.

To do so, they simulated the ageing process of the alloy by heat treating it for different periods. They documented how the microstructure changed during the ageing of the alloy using micrographs from the transmission electron microscope.

Whereas the classical two-phase microstructure consists of cuboid Y' precipitates embedded in a so called Y-matrix, during heat treatment, spherical Y particles initially form in the Y' precipitates of the alloy, then further coalesce into plates that finally split the Y' precipitates.

The thermo-mechanical properties of these types of alloys depend largely on the stability of this Y/Y' microstructure.

In order to determine the atomic constituents of the individual phases, but primarily to learn about the formation and make-up of the poorly understood Y particle, Vogel and Wanderka investigated the aged samples using atom probe tomography at the University of Munster.

They succeeded in reconstructing the atomic lattice of the samples layer by layer and determining the composition of all phases, so that they could explain the chemical evolution of the Y particles.

"Until now, it was assumed that splitting of the Y' precipitates refines the microstructure during ageing, which would be beneficial for the alloy's stability under thermo-mechanical load. We were able to show that this is not correct. The microstructure indeed changes considerably, but it is not improved by the splitting however.

"We were actually able to correlate the best mechanical properties with the presence of spherical or plate-like Y particles and not with the later stages after splitting of the Y' precipitates has taken place", explains Florian Vogel.

Nelia Wanderka adds: "If we want to improve the stability of the microstructure and thus the thermomechanical properties of the alloy, we need to be sure that the Y' precipitates are not split by the Y particles, but instead remain intact through appropriate heat treatment and composition of the alloy.

"Atom probe tomography helps us in understanding the role of the alloying elements in the formation and growth of the Y particles. From this, we can learn how to influence these processes."

The work was published 20 Dec 2013 in the distinguished journal Nature Communications. doi:10.1038/ncomms3955

.


Related Links
HZB Institute of Applied Materials
Space Technology News - Applications and Research






Comment on this article via your Facebook, Yahoo, AOL, Hotmail login.

Share this article via these popular social media networks
del.icio.usdel.icio.us DiggDigg RedditReddit GoogleGoogle




Memory Foam Mattress Review
Newsletters :: SpaceDaily :: SpaceWar :: TerraDaily :: Energy Daily
XML Feeds :: Space News :: Earth News :: War News :: Solar Energy News





TECH SPACE
What makes superalloys super - hierarchical microstructure of a superalloy
Berlin, Germany (SPX) Jan 21, 2014
Researchers have observed for the first time in detail how a hierarchical microstructure develops during heat treatment of a superalloy Materials in high-performance turbines have to withstand not only powerful mechanical forces, they also have to maintain their chemical and mechanical properties almost up to their melting points. For this reason, turbine manufacturers have employed specia ... read more


TECH SPACE
Boeing Joins BIOjet Team To Develop Biofuel Supply Chain In UAE

Renewable chemical ready for biofuels scale-up

UAE's Etihad demonstrates flight with biofuel mix

Boeing Finds Significant Potential in "Green Diesel" as a Sustainable Jet Fuel

TECH SPACE
Mideast looks at $50B to spend on solar power by 2020

From a carpet of nanorods to a thin film solar cell absorber within a few seconds

Solar-power device would use heat to enhance efficiency

DuPont Solamet Helps REC Increase Solar Panel Power Performance

TECH SPACE
France's Areva, Spain's Gamesa announce joint wind power venture

Musselroe Wind Farm provides fresh energy for local economy

Maine offshore wind project appears on track for federal funding

No Evidence of Residential Property Impacts Near Wind Turbines

TECH SPACE
Europe's 2030 climate targets get mixed reception

The German energy turnaround - implications for Russia

Global warming's biggest offenders

EU could cut emissions by 40 percent at moderate cost

TECH SPACE
EU issues framework for shale gas exploitation

Oil prices drop on China data

Shell to further scale down Australian operations?

Iran's oil minister to seek investment at Davos

TECH SPACE
ALMA Discovers a Formation Site of a Giant Planetary System

Herschel Telescope Detects Water on Dwarf Planet

Bright star reveals new exoplanet

'Dwarf planet' in deep space has water

TECH SPACE
Raytheon, L-3 demonstrate new ship protection system

Lockheed Martin Completes Critical Milestone to Upgrade US Navy's Electronic Warfare Defenses

China starts building second aircraft carrier

Vietnam takes delivery of its first 'black hole' sub

TECH SPACE
Mystery Mars rock reveals unexpected chemical composition

Mysterious stone 'rawled up' to Mars Rover Opportunity

Oppy Encounters A Surprise At Solander Point

Dutch researcher says Earth food plants able to grow on Mars




The content herein, unless otherwise known to be public domain, are Copyright 1995-2014 - Space Media Network. AFP, UPI and IANS news wire stories are copyright Agence France-Presse, United Press International and Indo-Asia News Service. ESA Portal Reports are copyright European Space Agency. All NASA sourced material is public domain. Additional copyrights may apply in whole or part to other bona fide parties. Advertising does not imply endorsement,agreement or approval of any opinions, statements or information provided by Space Media Network on any Web page published or hosted by Space Media Network. Privacy Statement